Dataset of ptychographic X-ray computed tomography of inverse opal photonic crystals produced by atomic layer deposition

Forskningsoutput: TidskriftsbidragArtikel i vetenskaplig tidskrift

Abstract

This data article describes the detailed parameters for synthesizing mullite inverse opal photonic crystals via Atomic Layer Deposition (ALD), as well as the detailed image analysis routine used to interpret the data obtained by the measurement of such photonic crystals, before and after the heat treatment, via Ptychographic X-ray Computed Tomography (PXCT). The data presented in this article are related to the research article by Furlan and co-authors entitled "Photonic materials for high-temperature applications: Synthesis and characterization by X-ray ptychographic tomography" (Furlan et al., 2018). The data include detailed information about the ALD super-cycle process to generate the ternary oxides inside a photonic crystal template, the raw data from supporting characterization techniques, as well as the full dataset obtained from PXCT. All the data herein described is publicly available in a Mendeley Data archive "Dataset of synthesis and characterization by PXCT of ALD-based mullite inverse opal photonic crystals" located at https://data.mendeley.com/datasets/zn49dsk7x6/1 for any academic, educational, or research purposes.

Detaljer

Författare
  • Kaline P Furlan
  • Emanuel Larsson
  • Ana Diaz
  • Mirko Holler
  • Tobias Krekeler
  • Martin Ritter
  • Alexander Yu Petrov
  • Manfred Eich
  • Robert Blick
  • Gerold A Schneider
  • Imke Greving
  • Robert Zierold
  • Rolf Janßen
Externa organisationer
  • Paul Scherrer Institute
  • University of Hamburg
  • Helmholtz-Zentrum Geesthacht
  • Hamburg University of Technology
  • National Research University of Information Technologies
Forskningsområden

Ämnesklassifikation (UKÄ) – OBLIGATORISK

  • Materialteknik
Originalspråkengelska
Sidor (från-till)1924-1936
Antal sidor13
TidskriftData in Brief
Volym21
StatusPublished - 2018 dec
PublikationskategoriForskning
Peer review utfördJa
Externt publiceradJa